Processing
Depending on the grade, Kalix® HPPA materials provide lower warpage, reduced shrinkage, and low to no flash. These improvements result in tighter dimensional tolerances and more cost-effective manufacturing due to fewer secondary operations such as deflashing.
Processing Guidelines | ||
Mold Temperature °C (°F) |
Melt Temperature °C (°F) |
|
Kalix® 9000 series | 80-120 (176-248) | 280-310 (536-590) |
Kalix® 2000 series | 80-120 (176-248) | 270-300 (518-572) |
Kalix® 5000 series | 115-130 (239-266) | 270-300 (518-572) |
Flash Measurements
Solvay internal test methods
Shrinkage
Solvay internal test methods